Usage of Sealants
Usage of Sealants [Nov 19, 2010]
Seaaring are strong adhensive,small shrinking,sofe from cracking,good for color fixing and decoration,anti-wearing,anti-virus,which makes it perfectly repare defects or cracks on floor surface.Oil painting can also be paved on sealant surface as it has nice water proof ability.
In order to achieve good effect,notes below shall be followed when utilizing:
1) Sealants can be utilized 7days after cement and tiles applied (you need to wait for 2 days when using int-erior wall tiles), operation temperature is no higher than 0 degree.
2) Firstly,tile or material surface as well as joint lines shall be cleaned,better use wet cloth to get the surface wet but without water on it in order not toprevent paintings and cements leaking into tiny holes on tiles,and to guarantee color attachment and final coagulation....
[ Click for details ]Sealant Operation Method [Nov 19, 2010]
Color difference may occur due to operation environment condition,mixed water quantity and operation me-thods.therefore,piease make decision after try sampies.
[ Click for details ]Crossline Location [Nov 19, 2010]
Crossline location can promote working efficiency,making tile pavement rapid and convinient;at the same time,it can also make tile gap even,tidy and beautiful,upgrading tile pavement effect.
[ Click for details ]Basement Settlement [Nov 19, 2010]
Grey gaps need cleaning,e.g.cracks,cement parts,water,etc,please wipe off ahead of time;if grey gaps are too dry,please humid them,and towards mulit-hole tiles (ceramic tiles), please get sealants gap wet ahead of time.
[ Click for details ]Quantity Calculation [Nov 19, 2010]
Sealant quantity differs according to tile dimension as well as width of tile gap.Please make sure by consu-Iting local dealers or company personnel.
[ Click for details ]Mixing Methods [Nov 19, 2010]
Normal:20kg with 5-6 litre water wide Gap:20kg with4-5litre wather Normal:5kg with2-3litre water wide Gap:5kg with1-2litre water
[ Click for details ]Mixing [Nov 19, 2010]
Put water into bucket,add powder sealants slowly,stur constantiy until they are well locater without grains,toothpaste like,and put aside quietly for5-10minutes,then stur slightly before use.
[ Click for details ]Grey Gap Pavement [Nov 19, 2010]
press even with grey gap knife before sealants get hard affter operation.
[ Click for details ]Cleaning [Nov 19, 2010]
Soaking water with foam to wipe off the dirts on tile surface when hardening.Ifhydrochloric acid has to be done for cleaning,please dilute it to 3%and immediately wipe it off with clean water after use in order to avoid remainings.Hydrochloric acid affect colors to some extent.
[ Click for details ]Notices [Nov 19, 2010]
1) repair and clean grey gap as soon as possible affter pavement
2) Operation can not be done in raining days or with acid cleaner.
3) The product is fixed,piease do not mix whit other materials that are not referred.